Discovery DSC 250 Differential Scanning Calorimeter

The DSC 250 differential scanning calorimeter measures heat flow with Tzero technology. Moreover, it covers -180 to 725 °C. Bargal supplies it in Israel.

  • Tzero heat flow technology
  • Temperature range from -180 to 725 °C
  • Modulated DSC for complex thermal events
  • Optional autosampler and refrigerated cooling
תיאור

The DSC 250 differential scanning calorimeter is a Discovery series instrument from TA Instruments. It measures heat flow with Tzero technology. As a result, it delivers a flat, stable baseline. In Israel, Bargal supplies the DSC 250.

Who is the DSC 250 for?

The DSC 250 suits labs that need accurate thermal data in daily work. It also suits teams that run many samples. Typical users include:

  • Polymer and plastics labs
  • Pharmaceutical and food laboratories
  • Materials R&D teams, as well as quality control
  • Labs that also run long autosampler routines
  • Universities that teach thermal analysis

Applications

  • Melting, crystallization and glass transition of materials
  • Complex thermal events, using modulated DSC
  • Heat flow measurements under controlled atmospheres
  • Unattended runs, especially with the optional autosampler
  • Sample imaging, as well as photocalorimetry with optional accessories

Why choose the DSC 250 differential scanning calorimeter?

  • Fusion Cell with Tzero heat flow keeps the baseline flat
  • Temperature range from -180 to 725 °C
  • Modulated DSC separates overlapping events
  • An app-style touch screen simplifies operation
  • Refrigerated cooling options reduce liquid nitrogen use
  • User replaceable cell and dual input gas delivery manifold
  • Optional photocalorimeter and microscope accessories
  • Tzero Press and pans speed up sample preparation

Technical specifications

Parameter DSC 250
Heat flow technology Tzero heat flow
Temperature range -180 to 725 °C (depends on the cooling accessory)
Baseline flatness (-50 to 300 °C) ≤10 μW (no baseline subtraction)
Baseline repeatability (-50 to 300 °C) <20 μW
Temperature accuracy ±0.05 °C
Temperature precision ±0.008 °C
Enthalpy precision ±0.08%
Modulated DSC (MDSC) Included
Autosampler Optional
Optional accessories Photocalorimeter, LED-PCA, microscope camera, optical accessory kit

 

Autosampler, cooling and accessories

The DSC 250 accepts an autosampler and several cooling options. Therefore, you can match the setup to your workload. In addition, the autosampler is optional on this model.

Moreover, you can read the full details on the official TA Instruments DSC 250 page.

Frequently asked questions

What is the DSC 250 differential scanning calorimeter?

It is a Discovery series DSC with Tzero heat flow and a Fusion Cell. Moreover, it measures thermal transitions from -180 to 725 °C.

What does Tzero technology do?

It measures cell resistance and capacitance. As a result, it gives a more accurate heat flow signal and a flat baseline. Therefore, you do not need baseline subtraction.

Can I add an autosampler?

Yes. An autosampler is available as an option. Moreover, refrigerated cooling keeps sub-ambient operation going during long autosampler runs.

Does the DSC 250 run modulated DSC?

Yes. Modulated DSC separates complex thermal events. In addition, it splits the signal into reversing and non-reversing heat flow.

How is it different from the DSC 25 and DSC 2500?

The DSC 250 offers Tzero heat flow. However, the DSC 25 uses standard heat flow, and the DSC 2500 adds advanced Tzero. In addition, only the DSC 2500 measures direct heat capacity.

 

Also see the Discovery DSC 25 differential scanning calorimeter.

For related measurements, see the Discovery DSC 2500 differential scanning calorimeter.

Also see the Discovery X3 multi-sample DSC.

Also see the DSC 25P pressure differential scanning calorimeter.

 

Interested in the DSC 250 differential scanning calorimeter? Send us an enquiry, and our team will respond quickly. We are also happy to discuss your samples and your application.

 

 

מכשיר ה-DSC 250 של TA Instruments: קלורימטר סריקה דיפרנציאלי עם טכנולוגיית Tzero וטווח טמפרטורות של 180- עד 725 °C למדידת התכה, מעבר זכוכית והתגבשות, באספקת ברגל ציוד אנליטי בישראל.

צרו קשר

היי! שמחים שהגעתם לאתר שלנו! באתר יש כרגע מאות מוצרים ואנחנו מוסיפים מוצרים כל הזמן. אם לא מצאתם את מה שחיפשתם או שאין לכם כוח לחפש (קורה לכולנו), כתבו לנו כאן מה המוצר שאתם מחפשים ונשלח אליכם הצעת מחיר/נחזור אליכם

    דילוג לתוכן